| Hard
Anodize with PTFE
Similar
to Hard Anodize per Mil-A-8625 except that PTFE such
as Teflon shall be applied onto the hard anodize finish.
Must pass 1,000 hours salt spray test.
|
| MIL-A-63576A
* |
Unless
otherwise
specified: |
| Type
I |
0.002"-
±0.0002" |
This
specification has a Type II (Thermoplastic resin) and
Type III (Thermoplastic resin) also, but they are not
currently available at Alexandria Metal Finishers. Note:
The 1,000 hour salt spray test is not a routine test
for Alexandria Metal Finishers. Please contact us as
to its availability. |
* This specification is provided for reference only,
as it has been cancelled. |