| Sulfuric
Anodizing
Color will vary with alloy. Aluminum with low alloying
elements will show practically no color change. Best
coating on aluminum for dyeing. Can be dyed practically
any color or shade
(Black, blue, red, gold, orange, green etc.).Salt
spray requirement is 336 hours
(5% NaCI solution) per method B-117 of ASTM. Minimum
weight for type II coatings:
Class 1-1,000 Milligrams/sq.ft.
|